SummarySulphide Stress Cracking (SSC) is a form of Hydrogen Stress Cracking (HSC). It is an environmental cracking mechanism that can initiate on the surface of high strength alloy steels or carbon steels containing localised areas of high hardness/stress.Your browser does not support PDF. Click here to download.