--- title: "Sulphide Stress Corrosion Cracking" slug: "sulphide-stress-corrosion-cracking" updated: 2026-10-27T23:12:43Z published: 2026-10-27T23:12:43Z canonical: "ims-handbook.cenosco.com/sulphide-stress-corrosion-cracking" --- > ## Documentation Index > Fetch the complete documentation index at: https://ims-handbook.cenosco.com/llms.txt > Use this file to discover all available pages before exploring further. # Sulphide Stress Corrosion Cracking ## Summary Sulphide Stress Cracking (SSC) is a form of Hydrogen Stress Cracking (HSC). It is an environmental cracking mechanism that can initiate on the surface of high strength alloy steels or carbon steels containing localised areas of high hardness/stress. [PDF document](https://cdn.document360.io/e492a0e0-a4ba-4aca-8fc6-76b95f91fdf3/Images/Documentation/CEN.16.10664 - Sulphide Stress Corrosion Cracking.pdf?sv=2026-02-06&spr=https&st=2026-10-28T13%3A39%3A02Z&se=2026-10-28T14%3A39%3A02Z&sr=c&sp=r&sig=zeEG2qe8%2BmHPzqIcc4n%2FLkkwjKzHX%2Fm7TM0g7hn9l4s%3D)