--- title: "Carbonate Stress Corrosion Cracking" slug: "carbonate-stress-corrosion-cracking" updated: 2026-10-27T23:12:43Z published: 2026-10-27T23:12:43Z canonical: "ims-handbook.cenosco.com/carbonate-stress-corrosion-cracking" --- > ## Documentation Index > Fetch the complete documentation index at: https://ims-handbook.cenosco.com/llms.txt > Use this file to discover all available pages before exploring further. # Carbonate Stress Corrosion Cracking ## Summary Carbonate stress corrosion cracking (also known as carbonate cracking or carbonate SCC) is a specific form of alkaline stress corrosion cracking that can occur in carbon steel and low-alloy steels exposed to alkaline aqueous solutions containing significant levels of carbonates. The cracking is predominately branched and intergranular, and typically occurs as a network of very fine, oxide-filled cracks that may be difficult to detect. [PDF document](https://cdn.document360.io/e492a0e0-a4ba-4aca-8fc6-76b95f91fdf3/Images/Documentation/CEN.16.10639 - Carbonate Stress Corrosion Cracking.pdf?sv=2026-02-06&spr=https&st=2026-10-28T14%3A21%3A46Z&se=2026-10-28T15%3A21%3A46Z&sr=c&sp=r&sig=E6gni6sbPjbEwWT68ACMjQKrINtMpXAVoSraSWNYwTA%3D)